Description / Abstract:
This method applies to hot-poured asphalt crack sealant used in the construction and maintenance of roadways.
The method covers the accelerated aging of hot-poured asphalt crack sealant material by means of elevated temperatures and vacuum as specified in MP 25 and PP 85.